LDPE Unfilled

Overview

What is the Material: LDPE Unfilled is a semi-crystalline material.

Key Material Features: This material is beneficial in applications requiring more flexibility than HDPE, while offering similar impact strength and chemical resistance.

Other Considerations: This material is attacked by strong oxidizing acids and UV light.

Physical

Property Value Typical ASTM Test
Chemical Designation (LDPE) Low Density Polyethylene
Color Natural White
Density (g/cm^3) 0.92 D 792

Mechanical

Property Value Typical ASTM Test
Modulus of Elasticity (Tensile Test) (psi) 57000 D 638
Tensile Strength at Break (psi) 100 D 638
Modulus of Elasticity (Flexural Test) (psi) 29000 D 790
Compression Strength: 10% Strain (psi) 1400 D 695
Compression Modulus (psi) 54000 D 695
Impact Strength (Izod) (ft-lbs/in) No Break D 256

Thermal

Property Value Typical ASTM Test
Deflection Temperature (°F) (264 psi) 116 D 648
Service Temperature Continuous (°F) 160

Electrical

Property Value Typical ASTM Test
Specific Surface Resistance (Ω/square) 1.00E13 D 257
Dielectric Strength (V/mil) 580 D 149
Dielectric Constant (1MHz) 2.28 D 150

Other

Property Value Typical ASTM Test
Moisture Absorption (%) (24 Hours) 0.01 D 570
Flammability HB
The data stated are typical values intended for reference and comparison purposes only. The data should not be used as a basis for design specifications or quality control. The information is provided as a guide to the best of our knowledge and given without obligation or liability. Testing under individual application circumstances is recommended.